jaw crusher esinga kukozesebwa nga coarse crusher ne medium crusher mu by’okusima eby’obugagga eby’omu ttaka, ebizimbisibwa, ebikozesebwa n’ebitongole ebirala. Okusinziira ku bugazi bw’omwalo gw’emmere, kigabanyizibwamu ebika ebinene, ebya wakati n’ebitono ebisatu.
Obusobozi: 100-1200TPH
Obugazi bw’omwalo gw’okuliisa bunene okusinga mm 600 ku byuma ebinene, obugazi bw’omwalo gw’okuliisa buli 300-600mm ku byuma eby’obunene obwa wakati, ate obugazi bw’omwalo gw’emmere buba wansi wa mm 300 ku kompyuta entono. Jaw Crusher nnyangu mu nsengeka, nnyangu okukola era eyesigika mu kukola.

Hot Tags .: jaw type crusher, China, abagaba, abakola, ekkolero, ekoleddwa mu China